Customization: | Available |
---|---|
Raw Material: | Chlorosulfonated Polyethylene |
Material: | Polyurethane Rubber |
Still deciding? Get samples of US$ 2.3/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
volatile% | Ch lorine content% | sulfur content% | Mooney viscosity ML1+4,100ºC | tensile strength% | elongation at break% | |
CSM20 | 1.5 | 27-31 | 1.3-1.7 | 23-33 | ||
CSM30 | 1.5 | 41-45 | 0.8-1.2 | 35-45 | ||
CSM40 | 1.5 | 33-37 | 0.8-1.2 | 3304 41-50 3305 51-60 |
25.0 | 450 |
CSM45 | 1.5 | 23-27 | 0.8-1.2 | 32-42 | 20.0 | 400 |
CSM4085 | 1.5 | 34-38 | 0.8-1.2 | 85-95 | 25.0 | 45.0 |
CSM6525 | 1.5 | 26-28 | 0.9-1.1 | 83-97 |